Nissan Terrano r20e. Manual — part 83
until the urethane adhesive has completely cured. Curing
time varies depending on temperature and humidities. The
curing time will increase under higher temperatures and
lower humidities.
WINDSHIELD, REAR SIDE WINDOW AND BACK DOOR
WINDOW
YBT078
WINDSHIELD AND WINDOWS
Removal and Installation (Cont’d)
BT-43
YBT079
WINDSHIELD AND WINDOWS
Removal and Installation (Cont’d)
BT-44
DRYING TIME FOR SEALANT
I
Reference: Time required for sealant to dry to desired hardness.
CAUTION:
Advise the user of the fact that vehicle should not be driven on rough roads or surfaces until sealant
has properly vulcanized.
Unit: days
Relative humidity
%
Temperature °C (°F)
Windshield and Rear window
Back door window
90
50
25
90
50
25
40 (104)
1.5
2.5
5.0
1.5
2.5
5.5
25 (77)
2.5
4.0
7.5
2.5
4.5
8.5
5 (41)
5.0
13.0
20.5
5.5
14.0
22.0
REPAIRING WATER LEAKS FOR WINDSHIELD
Leaks can be repaired without removing and reinstalling glass.
If water is leaking between the urethane adhesive material and
body or glass, determine the extent of leakage. This can be
done by applying water to the windshield area while pushing
glass outward.
To stop the leak, apply primer (if necessary) and then urethane
adhesive to the leak point.
SBF543B
WINDSHIELD AND WINDOWS
Removal and Installation (Cont’d)
BT-46